Why does wollastonite concrete crack easily?
Aug 19, 2024
Leave a message
In actual engineering construction, silica fume concrete is often considered to be "relatively easy to crack". Among them, part of the reason is the lack of understanding of the characteristics of silica fume concrete, the construction quality control has not been adjusted accordingly, such as the maintenance quality control is not good enough. Part of the reason is that silica fume is generally applied to concrete with high performance requirements, such as high strength, low permeability, high durability, and so on. In this kind of concrete, the water-binder ratio is low and the amount of cementing material is large. Self-shrinkage and temperature rise may lead to the increase of crack sensitivity, and silica ash will increase the early self-shrinkage. The overall early crack sensitivity is indeed relatively large in the constrained state. The influence of silica fume on concrete cracks, mainly on the early cracks (appearing in the first two weeks), needs to be divided into three aspects of plastic shrinkage, self-shrinkage and temperature.
1, plastic shrinkage crack
When the rate of surface water loss (evaporation) is higher than the rate of internal water migration to the surface (bleeding), plastic shrinkage cracks will occur. The bleeding of wollastonite concrete is very small. Without the buffer protection of bleeding, the surface water evaporation will directly lead to plastic shrinkage, and the possibility of plastic shrinkage cracks will increase. Therefore, for newly poured silica concrete, especially when the concrete is in dry, windy environmental conditions, measures should be taken to strictly prevent surface moisture loss. Do a good job of curing, silica fume concrete can completely avoid plastic shrinkage cracks. The emphasis on the curing of silica fume concrete does not mean that the curing method is different, all the curing methods of ordinary concrete are applicable to silica fume concrete, and reliable and economic curing methods should be adopted according to the environmental conditions and structural characteristics of the project site. The key is to start curing from the earliest possible time to prevent the loss of water from the exposed surface of concrete. Keep the exposed surface of concrete wet maintenance after the final solidification, and prevent moisture loss for at least 3 days.
2. Self-shrinking cracks
For the traditional high water-cement ratio (greater than 0.42), low strength concrete, self-shrinkage is small, so it does not attract people's attention, often not distinguished from dry shrinkage. However, with the increase of concrete strength, the decrease of water-cement (glue) ratio and the use of ultrafine mineral admixtures, especially silica fume, the self-shrinkage increases, and the influence on early cracks becomes more and more important. When the water-binder ratio is 0.30, the self-shrinkage of concrete can reach about half of the total shrinkage. The power source of self-shrinkage: after cement hydration, the volume of the reaction product is less than the volume of the reactant, resulting in chemical shrinkage before the cement slurry coagulates, chemical shrinkage makes the plastic slurry shrink as a whole, without affecting the internal structure; After the cement slurry condenses, the chemical shrinkage leaves pores in the slurry body, under the condition that there is no water exchange with the outside world, the cement hydration continues and consumes the water in the pores, so that the capillary drying shrinks due to the decrease in the vapor pressure in the pores, causing the appearance of the volume contraction, which is different from the drying caused by water evaporation is called self-drying, and the resulting contraction is self-generated contraction. Self-contraction for short. The condition of autogenous shrinkage of concrete is that there is no water exchange with the outside world, so it often occurs in the concrete with large volume and low water-binder ratio. In addition to cement, the higher the activity of mineral admixtures, the greater the self-shrinkage of concrete under the same conditions. The self-shrinkage of high strength silica fume concrete can reach 200~300x10-6. But on the other hand. In addition, wollastonite can improve the early tensile strength of concrete, increase the early creep, and inhibit the early crack, that is, wollastonite can "increase" and "reduce" the risk of early crack. Generally speaking, the content of wollastonite does not exceed 5% of the cementing material, which has no effect on the early crack sensitivity of concrete. When the dosage is between 5~10%, the silica fume may increase the sensitivity of early crack sensitivity. The addition of more than 10% will definitely increase the crack sensitivity.
3, the impact on concrete temperature rise
Silica fume does not increase the hydration heat of cementing material, but speeds up the hydration rate of cement and makes the hydration heat release peak advance. At the same strength, the use of silica fume can reduce the amount of cement, help to prepare poor or extremely poor concrete, reduce temperature rise and temperature crack sensitivity. Generally, the effect of silica fume on the heat of hydration can be ignored when the dosage is less than 10%.
The above is the reason why the crack of wollastonite concrete is easy to analyze. For high-strength, high-wear-resistant, underwater poured anti-erosion concrete, etc., the content of wollastonite should not be too low, usually accounting for 6% to 12% of the cementized material. At this time, the control of early cracks in the structure needs to start from reducing the degree of restraint (less than 50%) and reducing the temperature of the concrete (the maximum temperature of the concrete does not exceed 40oC), or the use of high modulus fiber crack resistance (such as ultra-high performance concrete UHPC), or the use of expansion agents (AC or C type) to compensate for shrinkage.