- The micro-silicon powder or silicon source (such as silicon tetrachloride) is evaporated into the reaction chamber.
- It reacts with oxygen or air at high temperatures to form an oxide of silicon (SiO₂).
- The silica particles generated by the oxidation reaction are deposited on the substrate surface or in the collection system at nanometer scale.
The basic method of preparing nano white carbon black by micro silicon powder: 2.Sol-gel method
- Microsilica powder is added to an appropriate solvent to form a silicon solution (usually a silicon source such as sodium silicate or tetraethoxysilane).
- Acidic or basic catalyst is added to promote the hydrolysis and condensation reaction of silicon source in solution to form silica sol.
- Nano-sized silica particles were formed by controlling the time and temperature of sol-gel reaction.
- After gelation, silica can be converted into nano white carbon black by drying, calcination and other processes.
- The microsilica powder is mixed with water or dilute acid solution and heated to a certain temperature (e.g. 180°C to 220°C) in a closed reactor.
- In high temperature aqueous solution, the silicon source dissolves and hydrolyzes to form SiO₂ nanoparticles.
- The silica obtained after the reaction can be filtered, washed and dried to obtain nano white carbon black.
- Micro-silica powder (or silane gas) is mixed with oxygen and sprayed into a high-temperature reactor.
- At high temperatures, the silicon source oxidizes to form SiO₂.
- The oxidized silica particles are deposited in nanometer form in the cooling area and collected by air flow.
- The microsilicon powder is mixed with a solvent (such as supercritical carbon dioxide) and treated under supercritical conditions.
- Under the action of supercritical fluid, the silicon source is hydrolyzed and converted into nano-silica.