The way to join is an element that many people ignore, but they do not know that the appropriate way to join can quietly improve the actual effect of carburization. When charging, the carbon raiser is stirred with the charge and placed in the bottom and middle of the induction furnace to achieve higher carburizing efficiency. At the time of addition, it is generally accompanied by other charges to join a piece, and the second furnace starts to invest in the remaining liquid iron 200-400KG on the plastic bag to put the carbon raiser into the iron level. In general, it is stipulated that every 100 kilograms of scrap steel is added to the carbon raiser 3-4KG, and this proportion is suitable for adding the carbon raiser. When the coreless induction furnace smelting steel casting, the target composition of cast iron, the preparation of various charges and other various processing factors all affect the carburizing efficiency of the carburizing agent.